ABS

1 Acrylonitrile Butadiene Styrene (ABS)

Info

While you are free to use any brand and type of material you wish on your AON3D machine, we can only provide support for AON3D-validated materials that we have tested and developed processes for in-house, all of which can be purchased from AON3D directly by contacting sales@aon3d.com.

1.1 General Process Settings

SettingValue
Extrusion Temperature220-250ºC
Bed Temperature100-120ºC
Chamber Temperature80ºC

1.2 Usage Notes

1.2.1 Build Surface Preparation

ABS prints best directly on Kapton tape. Wipe down the Kapton build surface with isopropanol before use. Larger prints and geometries especially prone to warping may require the use of Dimafix, an applied adhesion aid. A Dimafix Pen can be purchased from AON3D by contacting sales@aon3d.com.

1.2.2 Material Pre-treatment

ABS is mildly susceptible to hydration. When not in use, please store in a sealed package or container with dessicant. Support Material HIPS has excellent compatibility with ABS as a breakaway support material.

1.3 Sample Slicer Profiles

Single Extruder, 0.4mm nozzle: abs-sx-0.4mm

Dual Extruder with HIPS Support, 0.4mm nozzle: abs-dx-0.4mm

Single Extruder, 0.6mm nozzle: abs-sx-0.6mm

Dual Extruder with HIPS Support, 0.6mm nozzle: abs-dx-0.6mm

Did you find it helpful? Yes No